Description
Molecular Formula: C10H14O6
Molecular Weight: 230.21
Structural Formula:
Specification:
Items
Specifications
Boiling Point
267°C (lit.)
Density
1.19g/mL at 25°C (lit.)
Vapor Pressure
14hPa at 20°C(lit.)
Refractive Index
n20/D1.464(lit.)
Flash Point
>230°F
Acidity coefficient(pKa)
4.35±0.17(Predicted)
Color,Fe-Co
≤100
Acid value, mg KOH/g
200~300
Viscosity,cps at 25°C
100~200
MEHQ,ppm
350~450
Items | Specifications |
Boiling Point | 267°C (lit.) |
Density | 1.19g/mL at 25°C (lit.) |
Vapor Pressure | 14hPa at 20°C(lit.) |
Refractive Index | n20/D1.464(lit.) |
Flash Point | >230°F |
Acidity coefficient(pKa) | 4.35±0.17(Predicted) |
Color,Fe-Co | ≤100 |
Acid value, mg KOH/g | 200~300 |
Viscosity,cps at 25°C | 100~200 |
MEHQ,ppm | 350~450 |
Function:
1. Polymerization reaction function to form polymers with different properties, thus improving the physical and chemical properties of polymers.
2. It has a certain dilution ability, which can reduce the viscosity of the system and improve the fluidity and coating performance.
3. Reactivity function: it can react chemically with a variety of compounds to further modify and functionalize the material.
Application:
1. It can be used to manufacture high-performance coatings, such as UV curing coatings, etc., for the surface coating of wood, automobile, plastic, metal and other materials.
2. As an important part of UV curing ink, it can be cured quickly under ultraviolet light, which helps to improve the printing speed and productivity of the ink, and is widely used in paper, plastic, metal and other printing substrates.
3. Participate in the photopolymerization reaction, can significantly improve the adhesive bonding strength and curing speed, on a variety of materials such as glass, metal, plastic, rubber, etc. have shown good adhesive properties, to meet the adhesive needs of different industries.
4 can be used to modify a variety of polymer materials, can improve the flexibility of the material, toughness, adhesion and chemical resistance and other properties.